Patient Situation
Here’s what the dentist’s notes, scans and photos told us about this PFM crown molar remake :
The patient wanted a tooth-colored biting surface again and was fine with metal on the inside. They just didn’t want the new crown to break the same way.
What the Dentist Asked For
The Rx for this PFM crown molar, condensed :
The dentist also put the old crown in the box, so we could look at it, and added one note: “Please tell me if anything looks wrong before you start.”
What the Old Crown Showed Us
The chip
The bare metal at the bottom of the chip is the old coping, so the chip tells you how much porcelain sat on top of it. Our technician measured 2.6 mm from the chip floor up to the edge of the porcelain still standing on the buccal side of the ridge .
That’s thick. We keep posterior porcelain at 1.5–2.0 mm and even. Porcelain is strong when metal backs it up and weak when it’s left hanging. Ceramic can fracture if it isn’t properly supported by the metal framework, and a marginal ridge is about as exposed as a spot gets.
The coping shape
Through the chip, the old coping looked like a thin, even cap that followed the prep . Nothing rose up under the ridge. So the porcelain ridge stood on its own, with the palatal cusp of #4 landing on it every time the patient bit down.
We can’t prove that’s the only reason it broke. Bite force and a hard bite on something can play a part too. But the coping shape is the part a lab controls.
Was there room?
Room for porcelain wasn’t the issue here. A posterior metal-ceramic prep calls for 2.0–2.5 mm of occlusal clearance under porcelain and 1.0–1.5 mm under metal. We measured the new prep against the opposing scan and the bite :
| Area | Reading | Enough for porcelain? |
|---|---|---|
| Mesiobuccal cusp | 2.2 mm | Yes |
| Distobuccal cusp | 2.1 mm | Yes |
| Mesiolingual cusp | 2.0 mm | Yes |
| Distolingual cusp | 2.0 mm | Yes |
| Mesial marginal ridge (prep to planned ridge top) | 3.1 mm | Yes, with room to spare |
| Distal marginal ridge (prep to planned ridge top) | 2.9 mm | Yes, with room to spare |
That “room to spare” under the ridges is what matters most on a PFM crown on a molar. The prep drops off toward the proximal walls, so the marginal ridges have more height to fill than the cusps. If the coping stays flat, porcelain fills all of it.
PFM Crown Molar Options We Sent Before Making Anything
We sent the dentist a design screenshot, the chip measurement and three ways to build the new molar PFM crown :
| Option | What it means | The trade-off |
|---|---|---|
| A. Same outside shape, new coping | The coping rises under both marginal ridges so porcelain there stays 1.5–2.0 mm. Porcelain still covers the whole occlusal surface | No prep change and no visible metal. The ridges still carry porcelain, just backed by metal now |
| B. Option A, plus a metal mesial marginal ridge | The ridge and the mesial contact are metal, so #4 bites on metal there | Nothing left to chip at that spot, but a strip of metal shows when the patient opens wide |
| C. Metal occlusal surface | All the biting surface is metal, porcelain on the buccal only | Toughest of the three and needs the least room, but metal on the occlusal surface tends to show on lower teeth |
We can build all three. The patient had asked for a tooth-colored biting surface, so the dentist picked A .
They also asked for a metal coping try-in. The old crown had let food pack in, and they wanted to check the seat, the margins and the space over the coping in the mouth before any porcelain went on. They approved the design in our WhatsApp group the same day .
How We Made This Molar PFM Crown
Coping design
Metal coping
Our metal department cast the coping from the approved design . Before it left the lab, we checked its thickness with a caliper, looked at the margins under magnification for flash, and seated it on the printed model to make sure it didn’t press on the gums.
Coping try-in
The coping went to the clinic for the try-in. The dentist reported :
The dentist shipped the coping back with that bite record, and we kept going without changing the design.
Porcelain
The porcelain is matched to the alloy’s thermal expansion. The metal should expand slightly more than the ceramic, so the porcelain doesn’t end up in tension as it cools. Before the porcelain, the coping was blasted with aluminum oxide, cleaned ultrasonically and pre-oxidized so the porcelain bonds properly.
Then came opaque, then dentin and enamel porcelain in A3. The technician kept the layers even over the ridges and cusps, with no thick lumps over thin metal. We cap a PFM at three or four firings to keep the shape and color stable, and this crown took three . Each layer and firing went into the case record.
Final checks
Glazing and firing can move things a little, so we rechecked the contacts, bite and margins after the glaze. In a study of 3,750 single crowns, the remake rate was 3.8%, and proximal misfit, margin errors and esthetics were the most common reasons. So those get checked first.
Then we compared the crown with the approved design, and our QC technician signed it off against the Rx. It shipped in a foam-filled box.
Finished Result of the PFM Crown on a Molar
Here’s how this PFM crown molar case measured up at final inspection:
Seating feedback
The dentist: the crown seated with no margin changes. The mesial contact held floss with a firm snap, and one light touch on the distobuccal cusp needed adjusting .
The patient: the biting surface matches the teeth next to it, and food stopped packing at the two-week check .
Sending a Similar PFM Crown Molar Case
Remaking a molar PFM crown that chipped, whoever made it first? This is how it works with us. For the full range, see our PFM crowns and our PFM crowns for molars and premolars. If the bite is short, we also make a PFM crown with metal occlusal.
Every step happens in our own labs: four of them in Shenzhen and Huizhou, China, with about 460 people. CAD design, metal and porcelain work and QC all run in-house, and metal and porcelain work are kept apart in production. Istar is an FDA-registered establishment, Registration Number 3039441248, which you can check in FDA’s establishment database. The lab runs under ISO 13485.
Got a molar PFM crown that keeps chipping in the same spot? Send us the scan, photos of the old crown and your Rx. We’ll measure the space and send you design options before we make anything. Send your first case or talk to us.
FAQ
Can I send just one test case?
Yes, single trial cases are welcome. Ongoing partnerships suit a regular case flow best, since international shipping is the big cost on one-off cases.
Do I have to mail the old crown?
No. Photos and a scan taken before you remove it are usually enough to see where it broke. If you do have the crown, it’s worth putting in the box, because the chip lets us measure the porcelain over the old coping.
What can I adjust chairside, and when should I call you?
A slightly high bite is fine to adjust chairside. Polish the spot afterward so the surface stays smooth. If you see cracked porcelain, a crown that won’t seat or an open margin, stop and contact us.
If I've adjusted a crown and it still needs a remake, who covers it?
Usually we do. Send photos and tell us what you adjusted, and we’ll work out the cause with you.
Do you take rush cases?
Yes, at no extra charge, for clients who send 10 or more cases a month. We guarantee the ship date. The arrival date depends on customs, so we can’t guarantee that.