Dental Ceramics Lab Work, Planned From the Stump Up
An anterior crown that’s a shade off, or porcelain that chips a year after you seat it, costs you a second appointment and some of your patient’s trust. Istar Digital Dental Lab is a dental ceramics lab for clinics, DSOs and dental labs that want to send esthetic cases without that risk.
Our ceramists layer and characterize zirconia, pressed e.max and PFM restorations by hand, in our own labs in Shenzhen and Huizhou.
Ceramic Restorations From Our Ceramists
Seven kinds of work our dental ceramics lab makes, from fully layered anterior crowns to gingiva-colored porcelain.
Layered Zirconia
Porcelain built up by hand, layer by layer, over a zirconia framework: our fullest control of color, translucency and incisal detail. Best for: high-esthetic anterior crowns on a stable bite. → Zirconia Dental Lab
Micro-Layered Zirconia
A thin facial layer of porcelain over full-contour zirconia, pairing zirconia’s strength with surface depth and incisal effects that stains alone can’t give. Best for: anterior crowns that need strength and a natural look.
Stained and Glazed Zirconia
Monolithic or multilayer full-contour zirconia, characterized with stains and a glaze for efficient, strong restorations. Best for: posterior crowns and bridges, heavy bites and bruxism.
Pressed E.max
Lithium disilicate pressed with Ivoclar’s IPS e.max Press, then stained and characterized by hand. It’s the most translucent ceramic we make. Best for: anterior crowns, inlays and onlays. → E.max Dental Crowns and Bridges
Veneers
Thin pressed e.max veneers for esthetic cases, and zirconia veneers for patients with a heavier bite. Best for: discoloration, including fluorosis and tetracycline staining; enamel defects; anterior diastemas under 3 mm; minor malalignment; undersized teeth. → Veneers
PFM
Porcelain layered over a cast or milled metal framework, with a metal-free porcelain margin on request. Best for: posterior crowns and bridges, heavy bites and cost-conscious cases. → PFM Crowns & Bridges
Pink Porcelain
Gingiva-colored porcelain that rebuilds the soft tissue a case is missing. Best for: closing black triangles, covering recession and evening out an asymmetric gingival line.
Our layering porcelains come from Ivoclar, Shofu and Noritake. The material on your prescription is the material we use, and we never switch it without your consent.
How Our Ceramists Build a Layered Restoration
Esthetic failure is one of the three most common reasons dentists turn a crown away, alongside proximal misfit and marginal errors, according to a practice-based study of 3,750 single-unit crowns. Here’s how our dental ceramics lab keeps shade from becoming the reason one of yours goes back.
1. Planned From the Stump
The shade is built from what’s underneath, not from a tab.
- We read the stump shade first, then set the target shade.
- Masking takes its share of the thickness first. Whatever is left goes to dentin, enamel and opalescent layers.
- A dark stump or an uncoated metal post shows through zirconia. We’ll flag it and suggest an option.
- If the space is too thin for the shade change you’ve asked for, strength comes first: a stronger base, thinner porcelain and less incisal translucency. If a little more reduction would solve it, we’ll contact you before we start.
Your part: send photos of the prepared stump and the neighboring teeth, each with the shade tab in frame (Send a Case guide).
2. Layered for Light
Translucency, opalescence and fluorescence go where natural teeth have them.
- Dentin is cut back toward the incisal edge to leave room for translucent porcelain.
- Opalescent porcelain is confined to a thin incisal zone.
- Fluorescent porcelain sits in the dentin and tapers toward the edge.
- White spots, craze lines and translucent bands are copied from your photos.
Your part: if a characteristic is hard to describe, send a close-up of the neighboring teeth, or mail us the shade tab or an old restoration to match.
3. Fired Under Control
Few firings, and nothing ships on a contact the glaze has shifted.
- Color is compared before and after each firing.
- Porcelain usually goes through no more than three or four firings, with stepped heat-up, vacuum firing and slow cooling to avoid distortion and color drift.
- After the glaze firing, contacts, occlusion and margins are checked again, because glazing can shift them.
Your part: approve the design. Anterior veneer cases and multi-unit anterior ceramic cases get a design for your sign-off before production, and any other case can on request. Approval adds 1–2 working days.
4. Recorded for Next Time
Your next crown starts from this one’s recipe.
- For each layer, the technician records the porcelain, mix, placement and thickness, plus stain shades, dilution and firing parameters.
- Porcelains, stains and glazes are logged by batch and expiry date, used first in, first out, and never past date.
- Repeat work is made against your confirmed shade reference, photos and design files, with the material batch and firing parameters held, and each batch is checked against a reference sample.
- If an esthetic result is ever questioned, we can trace it from the shade records to the recipe, the material batch and the technician.
Your part: tell us once, in writing, how you like your shade, contour, contacts and surface texture. We apply it to every new case until you update it.
Keeping Porcelain From Chipping
Chipping is a common complication of both PFM and all-ceramic crowns, as the ADA’s overview of materials for indirect restorations notes. In our dental ceramics lab, most of the protection is decided before the first layer goes on.
Even, Supported Porcelain
On PFM work, we keep porcelain an even 1.0–1.5 mm on anterior teeth and 1.5–2.0 mm on posterior teeth, with no thick or thin spots. The metal framework is shaped to support the porcelain at connectors and wherever the bite lands.
Porcelain Matched to the Metal
The porcelain we choose expands slightly less than the alloy, so it isn’t left under tension as it cools. Metal surfaces are sandblasted, cleaned and pre-oxidized before the first layer, for a sound porcelain-to-metal bond.
Porcelain Only Where the Bite Allows
On a heavy bite, with bruxism or on a long span, layered porcelain carries more risk, and we’ll say so. We’ll suggest full-contour or micro-layered zirconia instead, which puts less porcelain in the path of the bite, or none at all.
If It Chips Anyway
Send photos of the chip when you report it. If the restoration seated well and only the porcelain failed, we remake it from the original data, so your patient doesn’t need a new scan or impression.
→ Full terms: Remake and Warranty Policy
Inside Our Dental Ceramics Laboratory
Porcelain work in our dental ceramics laboratory runs in its own area, apart from milling, printing and resin, to keep materials from cross-contaminating. Here’s who works on your cases there, and how we check what they make.
The People Who Layer Your Cases
Anterior esthetic cases go to our most experienced ceramists, and the most demanding ones go to the group leaders. New technicians train, assist experienced colleagues and retrain until they reach our skill standard before they work on cases alone.
A Ceramist You Can Reach
If a technician spots a margin, occlusion or material problem, they contact you by email or in your case group before going on. You can ask for a specific technician. Our four labs use nearly the same materials but have their own teams, so we can show you how they compare on your cases and keep your work with the one you prefer.
Checked Under Controlled Light
Shade is checked under a standardized light source, and translucency and fluorescence under backlight and UV. Final release is made by QC staff who don’t make restorations. They compare each restoration with your approved prescription and design, using a digital overlay on digital cases.
Istar Digital as Your Dental Ceramist Lab
If your lab designs or mills in-house but is short a ceramist, or needs overflow capacity in a busy month, use Istar Digital as your dental ceramist lab. Send us the stage you need: CAD design, milling, porcelain layering, porcelain additions and repairs, glazing or polishing. We accept editable exocad and 3Shape files.
A dental ceramist lab working behind yours has to stay out of sight. Finished work can ship straight to your dentist’s address. The waybill still shows our sender address, but we never contact your dentists, and we’ll sign an NDA.
When we work from a design you supplied, responsibility is split clearly. Send intraoral photos and the reason for the remake: chipped or cracked porcelain and a fractured crown or bridge are on us, while seating and occlusion problems are on your side.
Working With Our Dental Ceramics Lab
Start With One Anterior Case
The quickest way to judge a dental ceramics lab is a single anterior crown next to natural teeth, in layered zirconia, micro-layered zirconia or pressed e.max. Single trial cases are welcome; an ongoing partnership works best with a regular flow of cases.
Lab Time and Rush
Layered porcelain work, including layered and micro-layered zirconia, takes 3–5 working days in the lab. Routine crown and bridge takes 2–3. Days count from when complete records arrive, and time spent waiting on a design approval isn’t included. If you send 10 or more cases a month, rush service is free. We guarantee a rush case’s ship date; arrival depends on transit and customs.
Quotes and Price List
Quotes are itemized to your requirements, not bundled into one price. The number of units sets the base, the material sets the unit price, and design complexity adds to it. Your sales manager sends the current price list on request. You pay to send cases to us; we pay to ship finished work back, remakes included.
Credentials You Can Check
Istar Digital is an FDA-registered establishment, Registration Number 3039441248; look us up in the FDA establishment registration and device listing database. Our labs run an ISO 13485 quality management system, and restorations for the EU follow the MDR custom-made device procedure. You’re welcome to tour our dental ceramics laboratory in person or by live video.
Frequently Asked Questions
Which margin should we prepare for layered zirconia or PFM?
For layered zirconia, a shoulder. For PFM, a shoulder or a chamfer. Avoid knife-edge margins under porcelain, which are prone to chipping.
We adjusted a layered or e.max crown chairside. How should we finish it?
Polish the adjusted area with a Sof-Lex kit or flexible ceramic polishers, working from coarse to fine. Grinding removes the glaze, and a rough surface collects plaque. If you’d rather we refinish it, send it back: a small area can be reglazed locally, and a larger one gets a full reglaze or a step-by-step polish.
Which scan files should we send for anterior porcelain work?
A color PLY as well as the STL. The PLY carries the shade, surface texture and gingival color that our ceramists work from, which an STL doesn’t.
Send Your First Porcelain Case
Tell us your scanner, how many esthetic cases you send in a typical month and the porcelain work you prescribe most. If you’re a lab, tell us which stages you’d like to hand off. Your sales manager will reply and set up your account, so your first case reaches our dental ceramics lab with everything our ceramists need.